Both upper and lower platen have heating device and use oil hydraulic to compress. Pressure can be set 20%~90% of the full capacity. Place plastic or rubber material into the casting mold, grip it between upper and lower heating plate, apply pressure and certain temperature to form the material into a standard shape to be a sample to serve for test, or to be an example of color comparison, also to be example before mass-production.
| Specs | Description | |
| Capacity (Pressure) | 10Ton,30Ton, 50Ton | |
| temperature | Room temperature ~ 300℃ Heating speed :40℃-200℃ ,with 18 min Cooling speed:200℃-60℃, within 15 min |
|
| Optional device | Cooling water circulation system | |
| Timer | 0 ~ 999Minutes | |
| Platen Area | 30×30 cm | |
| Distance between heating platens | 120 mm (Max.) | |
| Attachment | Mold for forming specimen: 1Set | |
| Dimension | 110×70×152 cm(W×D×H) | |
| Weight | 320 kg (for 10 tons machine) | |